• +91 9810098570

  • info@realloyindia.com

realloy-C

An Universal CoCr bonding alloy compatible with all conventional ceramic materials

  • With a special composition
  • Can be melted with all casting methods
  • Also suitable for laser welding
  • Worldwide proven quality
  • Biocompatible
  • Excellent bonding with ceramics
  • Easy finishing and easy to polish after casting
  • Easy oxide removal after ceramic firing
  • Best in its class

COMPOSITION

Co 62.5% I Cr 24.6% I W 8.5% I Mo 2.9% I Si 1.3% I Nb, Mn, Fe, N < 1 %

This alloy is Nickel and Beryllium free and complies EN ISO 22674 Typ 4

PROPERTIES

  • Density
  • Vickers hardness
  • Linear CTE (25-500ºC)
  • Linear CTE (25-600ºC)
  • Melting interval
  • Casting temperature
  • Burning temperature
  • Proof strength (Rp 0.2)
  • Tensile strength (Rm)
  • Modulus of elasticity
  • Tensile elongation (A5)
  • 8,3 g/cm3
  • 285 (HV10)
  • 13.9 (10-6.K-1)
  • 14.0 (10-6.K-1)
  • 1304 - 1369 (ºC)
  • 1470 (ºC)
  • 980 (ºC)
  • 490 (Mpa)
  • 920 (Mpa)
  • 210 (Gpa)
  • 10 (%)